Mechanismof diesolderingduringaluminum diecasting
molten aluminum、critical temperature、die casting、intermetallic phases、ceramic coating、casting defect、phase diagram、liquid phase
TG146.21/TG249(金属学与热处理)
This research was sponsored by the North American Diecasting Association;the U.S. Department of Energy, Assistant Secretary for Energy Efifciency and Renewable Energy, Ofifce of Transportation Technologies, Lightweight Vehicle Materials Program, under contract DE-AC05-00OR22725 with UT-Battele, LLC. The author would like to thank E.A. Kenik and J. Song for scanning elect
2015-05-04(万方平台首次上网日期,不代表论文的发表时间)
共8页
136-143